Fa   |   Ar   |   En
   impact of tool-related parameters during fabrication of dissimilar aisi 1010 –cda 101 joints by fsw  
   
نویسنده basha k. anil ,sevvel p. ,giridharan k.
منبع scientia iranica - 2025 - دوره : 32 - شماره : 2 - صفحه:1 -14
چکیده    An experimental endeavor was made to determine suitable tool geometry and ideal values of travel speed, tilt angle, pin offset distance for fabricating 5 mm thick dissimilar aisi 1010 and cda 101 joints by friction stir welding (fsw). two differents sets of experiments were performed at constant 1200 rpm employing tools with distinct geometries and varying combinations of tool-related parameters. reports affirmed the attainment of flawless joints during 2nd set of experimentation by employing a cylindrical shouldered tool (25 mm in diameter) having a cylindrically tapered pin at 1200 rpm, 40 mm/min travel speed, by tilting the tool at 2 °, with its pin being inserted a 1.5 mm offset distance towardscda 101 plate. downward axial force of 7.214 kn was found to be ideal for joining these dissimilar metals and it was majorly influenced by the tool's travel speed and pin's offset distance. presence of different sized cu particles in aisi matrix, have led to the creation of brittle natured and large intermetallic amalgamations in nugget zone, thereby reducing the strength of fabricated defect-free weldment & leading to a diversified combination of brittle–ductile mode of fracture exhibiting a strength of 181 mpa.
کلیدواژه tool travel speed; pin offset distance; friction stir welding; tool geometry; tool tilt angle; aisi 1010; cda 101
آدرس grt institute of engineering and technology, department of mechanical engineering, india. , s.a.engineering college (autonomous), department of mechanical engineering, india. , easwari engineering college (autonomous), department of mechanical engineering, india.
پست الکترونیکی girimech4305@gmail.com
 
     
   