Fa   |   Ar   |   En
   vanadium extraction from a magnetite ore using alkaline roasting and acid leaching processes: optimization of parameters by response surface methodology  
   
نویسنده ghoddocy nejad d. ,taghizadeh m. ,khanchi a. r.
منبع journal of mining and environment - 2019 - دوره : 10 - شماره : 1 - صفحه:241 -255
چکیده    In this work, the alkaline roasting and sulfuric acid leaching processes were employed to extract vanadium from the magnetite ore of saghand mine in central iran. the response surface methodology based on the central composite design model was applied to optimize the parameters involved in the processes. the studied roasting parameters were temperature (900-1100 °c), sodium carbonate percentage (30-50 wt%), and time (13 h). in addition, the studied leaching factors included temperature (70-90 °c), liquidtosolid ratio (l/s) (5-20 ml/g), sulfuric acid concentration (2-6 m), and time (3-6 h). under the optimal conditions, the values for temperature, time, and sodium carbonate amounted to 1010 °c, 2.1 h, and 41 wt%, respectively, for the roasting process, while the values for temperature, l/s, sulfuric acid concentration, and time for the leaching process were estimated to be 85 °c, 12.4 ml/g, 4.25 m, and 4.7 h, respectively. under these conditions, about 83.8 ± 0.9% of vanadium was leached from the magnetite ore.
کلیدواژه magnetite ore ,vanadium ,alkaline roasting ,acid leaching ,optimization
آدرس babol noshirvani university of technology, chemical engineering department, iran, babol noshirvani university of technology, chemical engineering department, iran, nuclear science and technology research institute, iran
پست الکترونیکی akhanchi@aeoi.org.ir
 
     
   