   Optimized Leaching Conditions for Selenium from Sar-Cheshmeh Copper Anode Slimes  
   
نویسنده - - ,- -
منبع iranian journal of chemistry and chemical engineering - 2004 - دوره : 23 - شماره : 2 - صفحه:101 -108
چکیده    The recovery process of selenium from iranian sar-cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. the copper anode slimes are made up of those components of  the anodes, which are not soluble in the electrolyte. they contain varying quantities of precious metals like gold, silver, selenium and tellurium. they are being extracted as a by product in the copper production process.in this paper, some parameters affecting the leaching  conditions of anode slimes in nitric acid are studied. taguchi experimental design method is used to find out the effect of acid concentration, temperature and time.the statistical results of  the experiments show that the above parameters are important in the leaching of -10  microns fraction. the optimum conditions determined are: t = 90º c, acidity = 4 m and the leaching time = 60 min. under these conditions, 99 % of the selenium is leached out.    
کلیدواژه Sar-Cheshmeh mine ,Copper anode slimes ,Hydrometallurgy ,Selenium extraction
آدرس Mineral Processing Group, Tarbiat Modarres, Mineral Processing Group, Tarbiat Modarres University, P O Box 14115-143, Tehran, I R IRAN, ایران, Mining Department, Technical University of, Mining Department, Technical University of Shahrood, Shahrood, I R IRAN, ایران
 
     
   
Authors
  
 
 

Copyright 2023
Islamic World Science Citation Center
All Rights Reserved